Skip to main navigation Skip to search Skip to main content

Recent DIII-D progress toward validating models of tungsten erosion, re-deposition, and migration for application to next-step fusion devices

  • T. Abrams
  • , J. G. Guterl
  • , S. Abe
  • , D. C. Donovan
  • , I. Bykov
  • , C. A. Johnson
  • , J. H. Nichols
  • , J. D. Elder
  • , D. A. Ennis
  • , S. D. Loch
  • , D. L. Rudakov
  • , G. Sinclair
  • , C. H. Skinner
  • , P. C. Stangeby
  • , D. M. Thomas
  • , E. A. Unterberg
  • , W. R. Wampler

Research output: Contribution to journalArticlepeer-review

Abstract

Fundamental mechanisms governing the erosion and prompt re-deposition of tungsten impurities in tokamak divertors are identified and analyzed to inform the lifetime of tungsten plasma-facing components in ITER and other future devices. Various experiments conducted at DIII-D to benchmark predictive models are presented, leveraging the DiMES removable sample exposure probe capability and the Metal Rings Campaign, in which toroidally symmetric rows of tungsten-coated tiles were installed in the DIII-D divertor. In tokamak divertors, the width of the electric sheath is of the order of the main ion Larmor radius, and a vast majority of sputtered tungsten impurities are typically ionized within the sheath. Therefore, W prompt redeposition is mainly governed by the ratio of the characteristic ionization mean-free path of neutral tungsten to the width of the sheath. In-situ monitoring of the prompt redeposition of tungsten impurities in divertors is demonstrated via the use of WII/WI line ratios and the ionizations/photon (S/XB) method in L-mode discharges. Even with this relatively limited set of emission measurements, net erosion measurements were found to be a consistent upper bound to an analytic scaling based on the ratio of the W ionization length, λ iz , and the width of the magnetic sheath rather than the ratio of λ iz and the W+ gyro-radius. In the far-scrape-off layer (SOL) of the ITER divertor, however, it is calculated that the measurement of photon emissions associated with the ionization of tungsten impurities up to W 5 + may be required. Finally, W deposition patterns on DiMES collector probes, interpreted via DIVIMP-WallDYN modelling, reveal the key roles of progressive W erosion/re-deposition staps and E × B drifts in regulating long-range high-Z material migration.

Original languageEnglish (US)
Article number126503
JournalMaterials Research Express
Volume10
Issue number12
DOIs
StatePublished - Dec 1 2023

All Science Journal Classification (ASJC) codes

  • Electronic, Optical and Magnetic Materials
  • Biomaterials
  • Surfaces, Coatings and Films
  • Polymers and Plastics
  • Metals and Alloys

Keywords

  • DIII-D
  • divertors
  • erosion
  • re-deposition
  • sputtering
  • tokamak
  • tungsten

Fingerprint

Dive into the research topics of 'Recent DIII-D progress toward validating models of tungsten erosion, re-deposition, and migration for application to next-step fusion devices'. Together they form a unique fingerprint.

Cite this