A multitechnique surface analysis study of the adsorption of H2, CO and O2 on Bi Pt(111) surfaces

Mark T. Paffett, Charles T. Campbell, Rebecca G. Windham, Bruce E. Koel

Research output: Contribution to journalArticlepeer-review

34 Scopus citations

Fingerprint

Dive into the research topics of 'A multitechnique surface analysis study of the adsorption of H<sub>2</sub>, CO and O<sub>2</sub> on Bi Pt(111) surfaces'. Together they form a unique fingerprint.

Engineering & Materials Science

Physics & Astronomy

Chemical Compounds